弯钢化玻璃炸裂因素的探讨
免费下载
[全文大小:156 K]
单俊鸿[1,2] 张燕玲[3]
[1]河北工程学院,邯郸056038 [2]武汉理工大学硅酸盐材料工程教育部重点实验室,武汉 430070 [3]中国新型建筑材料工业设计研究院,杭州 310003
摘 要:
为了提高钢化玻璃的成品率,对炸裂这一影响弯钢化玻璃成品率的主要因素进行了探讨,发现玻璃结构,结石、钢化工艺(加热,压弯、冷却)等是影响弯钢化玻璃成品率的主要因素。[著者文摘]
文章出处:
《山东建材》-2005年26卷5期 -35-37页
Shandong Building Materials
栏目信息:
分 类 号:
文献标识码:
A
文章编号:
1003-1324(2005)05-0035-03
[参考文献]
The discussion of crack factors of curved toughened glass
Shan Junhong, Zhang Yanling ( 1. Hebei University of Engineering Handan China; 2. Wuhan University of technology Wuhan China; 3.China new building materials industry Hangzhou institute Hangzhou China )
Abstract:
The crack reasons of curved toughened glass have been discussed for improving the rate of finished products of curved toughened glass. It has been found that glass structure; concretion and tempering technology (such as heating; press bending; cooling) are main factors that affect the rate of finished products of curved toughened glass.[著者文摘]
Key words:
crack; glass; glass structure; concretion; bending and tempering technology