摘 要:
通过对链条用40Mn带钢淬火硬度不均的调查分析,认为C、Mn含量低及用户不合适淬火工艺是淬火硬度不均的主要原因,为此针对厚规格链片开发40Mn-1,并协助用户调整淬火工艺。[著者文摘]
文章出处:
《河南冶金》-2007年15卷B09期 -25-28页
Henan Metallurgy
栏目信息:
分 类 号:
相关文章:
RESEARCH AND ANALYSIS OF NON -UNIFORM QUENCHED HARDNESS OF 40Mn STRIP USED FOR CHAIN
Hu Xiaotang, Mao Weidong (Echeng Iron & Steel Company, Wu Steel)
Abstract:
The research was carried out on non - uniform quenched hardness of 40 Mn strip used for chains. The results shows that lower C、Mn contents and the wrong quenching process were main causes. 40 Mn - 1 was developed for thickness chain and quenching process was adjusted.[著者文摘]
Key words:
quench; non -uniform hardenss